Product family
HASTELLOY® S alloy
Made by Haynes International, INC · Kokomo, IN
- Iron
- 3%
- Cobalt
- 2%
- Nickel
- balance%
- Silicon
- 0.4
- Chromium
- 16%
- Material
- HASTELLOY S
- Max temp c
- 900
- Max temp f
- 1650
- Molybdenum
- 15%
- Applications
- seal‑ring
- Test period h
- 1000
- Metal affected mm
- 0.19
- Metal affected mils
- 7.5
From Haynes International, INC’s own documents · read October 12, 2026 · not verified by FactoryRegistry
Documents
Where this comes from — 5 documents
A machine read this from documents Haynes International, INC publishes on its own website, as of October 12, 2026. FactoryRegistry has not verified it; the documents are the authority.
- “THE AMERICAN SOCIETY OF MECHANICAL ENGINEERS, page 2: “Alloy S possesses a useful combination of properties”
- “THE AMERICAN SOCIETY OF MECHANICAL ENGINEERS: “THE AMERICAN SOCIETY OF MECHANICAL ENGINEERS”
- EPD Congress 2003 Edited by M, page 8: “HASTELLOY S alloy … low thermal expansion alloy … used in seal rings.”
- EPD Congress 2003 Edited by M: “EPD Congress 2003 Edited by M”
- HASTELLOYSalloy: “HASTELLOYSalloy”
- HASTELLOYXalloy, page 11: “max_temp_f: 1650”
- HaynesInternationalAerospaceAlloys, page 1: “HASTELLOY® S alloy”
- HaynesInternationalAerospaceAlloys: “HaynesInternationalAerospaceAlloys”