FactoryRegistry
Claim a page

Product family

HASTELLOY® C‑22HS® alloy

Made by Haynes International, INC

Iron
3%
Boron
0.015%
Carbon
0.02%
Cobalt
2%
Nickel
61
Silicon
0.4%
Aluminum
0.25%
Chromium
16%
Tungsten
1%
Lanthanum
0.02%
Manganese
0.5%
Treatment
2 steps: 16 h at 1300°F (704°C), furnace cool to 1125°F (607°C), hold 32 h at 1125°F, air cool
Molybdenum
15%
Nickel percent
61

From Haynes International, INC’s own documents · read October 12, 2026 · not verified by FactoryRegistry

Documents

Where this comes from — 10 documents

A machine read this from documents Haynes International, INC publishes on its own website, as of October 12, 2026. FactoryRegistry has not verified it; the documents are the authority.